A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Problem with oxygen plasma bonding of two pdms slabs
Problem with oxygen plasma bonding of two pdms slabs
2009-04-09
김태진
2009-04-10
Debkishore Mitra
2009-04-11
김태진
2009-04-12
Lukas Bogunovic
Problem with oxygen plasma bonding of two pdms slabs
김태진
2009-04-09
Hi all!

I've been trying to bond two pdms devices using an oxygen plasma source.

It seems that the plasma system can effectively bond two untreated pdms slabs,
but the problem is...

I have to coat my patterned wafer with silane as it has small pit/trench
features.

After slicing up my pdms slabs, I immediately tried bonding these two slabs
together but without success.

The plasma system has no problem in bonding two untreated pdms slabs, so I
anticipate that the silane has rendered the pdms hydrophobic, leading to a
failure in bonding.

Is there a way to remove the silane coated pdms, after peeling it off from my
wafer, to enhance the bonding strength?

Thank you!

Best,

TJ
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Mentor Graphics Corporation
University Wafer