Tommy,

It has been a while since I worked with polysilicon, so I am
giving these numbers to you without further cheching my memory:
Depending on process condition, I used 140GPa for Young's
modulus. Sometimes that number can go up to 170GPa. Most solid
has Poisson's ratio of 0.3 so that's the number I used. More than
a few mems paper in the early 90's reported on Young's modulus
measurements.

Patrick Cheung, research scientist   Xerox PARC, MS 35-1674
(O) 650-812-4338 (FAX) 650-812-4334   3333 Coyote Hill Road
[email protected]                  Palo Alto, CA 94304
>>                                                       >>
>>                                                       >>

On Thu, 17 Sep 1998, Tommy Roussel wrote:

This is a multi-part message in MIME format.

------=_NextPart_000_0001_01BDE299.AFA2D600
Content-Type: text/plain;
        charset="iso-8859-1"
Content-Transfer-Encoding: 7bit

I was wondering if anyone could give me the material properties of
polysilicon.  I have found the pre-formed properties (solubility, etc) but
can't seem to locate Young's modulus or Poisson's ratio.

Thanks,

Tommy Roussel
[email protected]
http://www.ifm.latech.edu

------=_NextPart_000_0001_01BDE299.AFA2D600
Content-Type: text/html;
        charset="iso-8859-1"
Content-Transfer-Encoding: quoted-printable









I was=20 wondering if anyone could give me the material properties of = polysilicon. =20 I have found the pre-formed properties (solubility, etc) but can't seem = to=20 locate Young's modulus or Poisson's ratio.
 
Thanks,
 
Tommy = Roussel
[email protected]
http://www.ifm.latech.edu
------=_NextPart_000_0001_01BDE299.AFA2D600--
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Tanner EDA by Mentor Graphics
The Branford Group