MEMSnet Home: MEMS-Talk: scratch and dig specs for anodic bonding
scratch and dig specs for anodic bonding
2009-04-28
Robert MacDonald
2009-04-28
Mehmet Aykol
2009-04-30
[email protected]
2009-04-30
Shay Kaplan
scratch and dig specs for anodic bonding
Mehmet Aykol
2009-04-28
I remember a number 15nm as the average roughness for the limit but I might
be wrong. I am sure you can google it and find enough resources about it.
Also if you are using Pyrex from wafer companies like university wafer or
any other company they usually stock only polished Pyrex wafers.

Mehmet

On Tue, Apr 28, 2009 at 1:29 PM, Robert MacDonald <
[email protected]> wrote:

> Does anyone have standard specifications for pyrex wafer surface finish to
> achieve a good hermetic anodic bond to Si (assuming good conditions).
>
> In particular, I'm looking for a scratch and dig spec, or a surface
> roughness specification.
>
> Thanks,
>
> Rob MacDonald

--
Mehmet Aykol
University of Southern California
EE - Electrophysics
Phone: (213) 821-4090
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Nano-Master, Inc.
University Wafer