MEMSnet Home: MEMS-Talk: Stainless etchant
Stainless etchant
1998-10-12
Sangwook Lee
Stainless etchant
Sangwook Lee
1998-10-12
Hi!
I am wondering if someone has some information about stainless steel
etchants, or vendors. We are going to etch 200 um thick stainless steel.
The stainless steel has some of Cr and Ni. We tried some etchants
followed by a Metal Handbook. But the etch rate is not fast enough.
I heard ferric chloride can etch the stainless steel. But I don't have
the information about the concentration. If you give us some information,
We will really appreciate that.

Sang-Wook


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing