Bearing holes in pyrex/glass wafers
2009-05-01
김태진
2009-05-01
Mehmet Aykol
2009-05-01
Kirt Williams
2009-05-02
Brian Stahl
2009-05-02
[email protected]
2009-05-02
Xiaoguang Liu
2009-05-02
Jackgong Hotmail
2009-05-02
HENRI FLECHNER
2009-05-03
Jackgong Hotmail
2009-05-04
Fei Wang
2009-05-04
Robert MacDonald
2009-05-06
김태진
2009-05-04
%Mihaela Carp
2009-05-02
HENRI FLECHNER
2009-05-03
tarun mudgal
2009-05-05
Jackgong Hotmail
2009-05-04
Tomblin, Graham
Bearing holes in pyrex/glass wafers
tarun mudgal
2009-05-03
hi

I have been drilling holes in glas wafers for microfluidic devices.
i am using an ultrasonic driller and alongwith the driller we just run water
solution having SiC powder. it takes hardly 1-2 minutes for 0.5 mm glass
wafer

maybe you could use that

thnx
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Harrick Plasma, Inc.
Nano-Master, Inc.