Hi Ben Pepin,

The thickness depends on the material you want to deposit on a given
substrate and the quality of deposit you would like to achieve. I have
deposited about 10 microns gold on a silicon substrate patterned with
a Chromium-Gold seeding. There might be a thicker deposit than what I
have mentioned but then again it depends various process variables, coat
quality, material deposited and the substrate.

Regards,
Prasanna

On Mon, May 25, 2009 at 6:21 PM, Ben Pepin  wrote:

> Hello,
>
> I am an undergraduate research student at Mizzou and was wondering how
> thick
> of a coat you can achieve from electroplating? I am trying to get as thick
> of a coat as possible and would appreciate any tips or suggestions.
>
> Thanks,
> Ben Pepin
> [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Mentor Graphics Corporation
University Wafer