Don Friedrich
Estimate mechanical properties of Novolac PR films
Don Friedrich
2009-06-12
I need an estimate of Young's modulus (E) and the coefficient of thermal
expansion (CTE) of Novolac based positive PR films of thickness 3-10 um.
The AZ9000 series PR would be a good example.

In particular I need an estimate for such films after softbake (90-100C)
and also after mild hard bake (around 115-120C).  The estimate can be
very approximate.

If you know some values or could point me to a reference with this
information, I would be grateful.

Thanks -
Don Friedrich
JDSU - Applied Optical Technologies
Santa Rosa, CA
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
University Wafer
Tanner EDA by Mentor Graphics