Yongliang Yang
2009-06-20
Maybe the primary falt is along <211> direction.

you can etch the wafer in KOH with rectangle mask to determine the crystal
direction.

2009/6/7 Andrea Mazzolari 

> Hi all,
>
> which are the cleaving planes for (110) wafers ?  I've tried to find this
> info on the web, but was not able :(
>
> Thanks,
> Andrea
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
University Wafer