2009-07-06
Leon Maurer
2009-07-06
Joseph Grogan
2009-07-06
Felix Lu
2009-07-06
Bill Moffat
2009-07-08
Leon Nathaniel Maurer
2009-07-08
Felix Lu
2009-07-08
Brubaker Chad
Al-Si wafer bonding
Bill Moffat
2009-07-06
Leon,

     Plasma bonding is a relatively low temperature operation.  Think up
to 50 degrees C.  I know that silicon wafers can be successfully bonded.
Not sure about Sapphire, Aluminum, Silicon but we could do tests for
you.  Bill Moffat

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Leon Maurer
Sent: Monday, July 06, 2009 7:42 AM
To: [email protected]
Subject: [mems-talk] Al-Si wafer bonding

Howdy,

I'm looking for information on Al-Si wafer bonding, and I saw a good
thread here from 2002 about why I don't want to do it, so I was
wondering if there was equally good information here about how to do it
if I had to.

I'm new to wafer bonding, and the papers I've found that mention it
haven't been too informative (although perhaps I haven't found the right
papers). One issue is that the wafer bonding setup I have access to only
goes up to 550C, and for various reasons (including that we'd eventually
like to bond sapphire to Si with an intermediate Al layer
-- my understanding is that the differences in thermal expansion rates
can cause trouble) we'd like to avoid temperatures that high.

We don't need particularly strong bonding -- mostly it just has to
survive (man)handing during the rest of fabrication (which will involve
some lithography and etching). However, the bond or two I've made so far
aren't cutting it (200C, 2.5MPa, 30min, they fail if you look at them
funny). Anyone know what strengths can be achieved at different
temperatures/pressures/times? Any tricks that could make things go more
smoothly? Other advice?

Thanks.
-Leon
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics
Nano-Master, Inc.