A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Peel off PDMS
Peel off PDMS
2009-07-09
Shah, Forum N
2009-07-09
[email protected]
2009-07-10
Shah, Forum N
2009-07-11
Andrew Sarangan
2009-07-13
Shah, Forum N
2009-07-09
Andrew Sarangan
2009-07-10
Shah, Forum N
2009-07-10
Liang Zhao
2009-07-11
Barbara Cortese
Peel off PDMS
Shah, Forum N
2009-07-13
Thanks Andrew. I went through the product details but it says it shows good
results with glass substrate. Have you used it with Silicon wafer as a
substrate?

-----Original Message-----
From: Andrew Sarangan [mailto:[email protected]]
Sent: Friday, July 10, 2009 11:57 PM
To: General MEMS discussion
Subject: Re: [mems-talk] Peel off PDMS

You might be thinking of silane gas, which is different from the
liquid materials used to silanize the surface. You could use Trichloro
trifluoro propyl silane (from Sigma), or Sigmacote, or Jerseycote. You
can wet the surface with this material, or spin coat, or put it in a
dessicator and pull a vacuum to evaporate it. I don't think the
application method is that critical. We've tried Jerseycote and it
works well.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation