MEMSnet Home: MEMS-Talk: Si Deep RIE with AZ9260 mask
Si Deep RIE with AZ9260 mask
2009-07-20
Taekyung Kim
2009-07-20
shay kaplan
2009-07-20
Xiaoguang Liu
Si Deep RIE with AZ9260 mask
Taekyung Kim
2009-07-20
Hello folks,

I'm trying to do Si deep RIE with AZ9260 photoresist as a mask in a
PlasmaTherm etcher.
Any good recipe for AZ9260 PR?

The recipe I used was as follows.

1. AZ9260 spun at 2000 rpm for 60s (~11um)
2. 110C 5 min softbake
3. 540mJ/cm2 exposure
4. AZ 421K developer ~3min
5. No hardbake.

The smallest feature size is 20 un wide lines.

The mask would barely hold up to 200 cycles of etching.

Thanks

TK
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing