A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: microfabrication of blade structures
release of metal structures and etching of stainless steel
2009-07-28
Robert Fahey
microfabrication of blade structures
2009-07-28
Robert MacDonald
2009-08-03
Chilcott, Dan - NV
2009-07-28
Robert MacDonald
microfabrication of blade structures
Robert MacDonald
2009-07-28
Rob,

I've had some success fabricating blades out of 100 Si using a KOH etch. This
may be a good place to start.

Rob MacDonald
Shearwater Scientific

Robert Fahey writes:

Hi All

i'm looking into possible methods of using microfabrication methods to fabricate
blade or cutting structures. I was wondering if anyone on here has any
suggestions or knows of any similar work that has been carried out in the past?

I was thinking of using KOH etching of <100> Si wafers and use the natural
54.7degree angle as a cutting edge. Can I treat the Si in any way to make the
cutting edge harder? Does anyone have any experience on the use of silicon
carbide/tungsten carbide/similar materials for hardening purposes?

Does anyone have any other suggestions? I would also be keen to explore options
in metals.

thanks
Rob
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Harrick Plasma, Inc.
Mentor Graphics Corporation