about platinum etching
2009-08-08
abhaya joshi
2009-08-10
Yoshi.Sakata_Gmail
2009-08-10
Bill Moffat
2009-08-10
walter
2009-08-10
Miyakawa, Natsuki
about platinum etching
Bill Moffat
2009-08-10
Questions, Are you vacuum vapor priming, soft baking, and hard baking?
If so what temperatures are you using?  What photo resist and how long
is the etch?

Bill Moffat

________________________________

From: [email protected] on behalf of abhaya joshi
Sent: Sat 8/8/2009 7:25 AM
To: [email protected]
Subject: [mems-talk] about platinum etching

hi,

i am doing platinum etching (200nm). i am using HCL (8):HNO3 (1)
solution at 70C>

i am observing lot of non uniform etching behavior and lot of
undercutting.

can any one suggest how to avoid this.

-abhay joshi
university of pune
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Nano-Master, Inc.
Addison Engineering