Shao Guocheng
2009-08-11
Bill Moffat
2009-08-12
Shao Guocheng
2009-08-12
Bill Moffat
2009-08-17
Andrew
2009-08-17
Bill Moffat
2009-08-17
Bill Moffat
HDMS treatment of SU8 mold used for PDMS thin film fabrication
Shao Guocheng
2009-08-11
Hi, Guys,

    I'm trying to make some PDMS thin film about 40um thick. Without using any
anti-sticking agent, I'm able to get the film with small size, but have hard
time obtain bigger piece. So I'm thinking about doing silanization treatment for
my SU8 mold. We have HDMS available in our lab. Can any one share some
experience about SU8 mold silanization. what kinda protocol should I take, any
special precautions because from what I know, HDMS is toxic, although maybe not
as bad as some other silane like TMCS.   thx

Shao



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing