MEMSnet Home: MEMS-Talk: Gold peel off with PMMA mask
Gold peel off with PMMA mask
2009-08-18
luhaorice
2009-08-18
Ruiz, Marcos Daniel (SENCOE)
2009-08-19
luhaorice
2009-08-19
Ruiz, Marcos Daniel (SENCOE)
Gold peel off with PMMA mask
luhaorice
2009-08-18
Dear all,

we created patterns on SiO2 with Cr and Au(etching process).  Then, PMMA
was spin coated on the chip followed by EBeam lithography to create a
few windows on PMMA.  We etched part of SiO2 in diluted HF(5:50ml) for
5mins.  After removing PMMA in acetone, we found all fine gold
structures peeled off even under areas protected by PMMA.

Could I have some suggestions to solve it please?

Thanks,
Hao
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
MEMS Technology Review
Process Variations in Microsystems Manufacturing