A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: thermally curable glue
thermally curable glue
2009-08-11
Ulli Hansen
2009-08-11
Brian Stahl
2009-08-13
Kuijpers, Peter
2009-08-14
Fei Wang
2009-08-14
Kuijpers, Peter
2009-08-17
Roger Shile
2009-08-18
Kuijpers, Peter
2009-08-18
Roger Shile
thermally curable glue
Roger Shile
2009-08-18
Peter,

A Google search for Hitachi dry film DFXP10050C1 came up empty.  Is this
film designed for wafer bonding?

Roger Shile

-----Original Message-----
Subject: Re: [mems-talk] thermally curable glue

Hello,

I'm sorry. It wasn't Fuji, but Hitachi dry film.
We used DFXP10050C1.

Regards,

Peter Kuijpers

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Addison Engineering
MEMS Technology Review