A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: SU8
SU8
2009-09-08
renil kumar
2009-09-08
Bob Henderson
2009-09-08
Yu Wang
2009-09-08
Bob Henderson
2009-09-11
Maria Matschuk
2009-09-11
Bob Henderson
2009-09-15
eowin rohan
2009-09-15
Gareth Jenkins
2009-09-15
James Paul Grant
2009-09-15
Bob Henderson
2009-09-16
Brubaker Chad
2009-09-21
James Paul Grant
2009-09-15
Barbara Cortese
SU8
Bob Henderson
2009-09-08
Ken:

I have used SU-8 for DRIE and found it to have much higher selectivity than
standard positive photoresist. We were able to pattern an SU-8 formulation
that was only 5 microns thick and do DRIE without cross-linking thus we were
able to ash the photoresist off after etch. It worked well.

Bob Henderson

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of renil kumar
Sent: Tuesday, September 08, 2009 3:42 AM
To: [email protected]
Subject: [mems-talk] SU8

Hi All,
                   Does anyone know the selectivity between SU8 and Silicon
in DRIE environment. can i use SU8 as a hard mask during DRIE process. I
want to etch 30 um down to the silicon wafer to form 1.2 um thick vertical
walls for that i am using e-beam lithography. i will be grateful for any
suggestion regarding this. thanking you.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing