MEMSnet Home: MEMS-Talk: Modifiy hydrophobic glass surface to hydrophilic?
Modifiy hydrophobic glass surface to hydrophilic?
2009-09-08
Xu, Wenwei
2009-09-08
Bill Moffat
2009-09-08
Andrew Sarangan
Modifiy hydrophobic glass surface to hydrophilic?
Bill Moffat
2009-09-08
Are you sure you want to move from hydrophobic to hydrophilic.
If so Plasma.

Bill Moffat

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Xu, Wenwei
Sent: Tuesday, September 08, 2009 8:41 AM
To: [email protected]
Subject: [mems-talk] Modifiy hydrophobic glass surface to hydrophilic?

Hi Guys,

Anyone know an easy way to change the surface properties of glass from
hydrophobic to hydrophilic?

Thanks
Wenwei
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
Nano-Master, Inc.
Harrick Plasma, Inc.