Photo resist is sensitive to U.V. light.  There is about 2% U.V. in
normal white light which makes resist sensitive to white light.  If you
use normal precautions you can expose resist with white light just
expect a long exposure time.  Bill Moffat

________________________________

From: [email protected] on behalf of Seung-Hoon Kim
Sent: Thu 10/22/2009 7:45 PM
To: [email protected]
Subject: [mems-talk] Photoresist sensitive to visible wavelengths

Hi all,

I am searching for a photoresist that is sensitive to visible wavelength
of light.

especially in 600-800 nm region. I found a conference paper in which
SU-8 3050BW.

a photoresist sensitive to visible range of light, was used. However, I
could not find any information about SU-8 3050BW.

Or is it possible to modify conventional photoresist to be sensitive to
visible spectrum by using photoinitiator and photosensitizer?

Thanks,

Kim, Seung Hoon
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering
Tanner EDA by Mentor Graphics