wet etch of 2um Si3N4
2009-10-30
Nor Hafizah Ngajikin
2009-10-30
Kuijpers, Peter
2009-10-30
Shivalik Bakshi
2009-10-31
Edward Sebesta
2009-10-31
xudehui0108
wet etch of 2um Si3N4
xudehui0108
2009-10-31
Is the nitride has experienced a thermal oxidation process? If so, there will be
a thin oxide in the surface. This thin oxide should be etched prior to the
nitride etching.
Additionally, 1 hour H3PO4 etching is not enough to remove 2 micron Si3N4.

2009-10-31
xudehui0108


发件人: Nor Hafizah Ngajikin
发送时间: 2009-10-30  14:35:53
收件人: mems-talk
抄送:
主题: [mems-talk] wet etch of 2um Si3N4

Dear all,

I've tried to etch 2 micron thickness of Si3N4 using hot H3PO4. The
concentration of H3PO4 is 85w%. I heat the H3PO4 at 150 degree celcius for 1
hour. Unfortunately, this experiment didn't work as expected. None of the
nitride is etch away.

Can anybody share with me your experience on nitride etch using H3PO4.

Thank you.

Hafizah

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Mentor Graphics Corporation
MEMStaff Inc.