I am doing a research on BMI. I need to coat a film (5um to 10 um) on Si
wafer.

Can anyone recommend a suitable solvent for dissolving BMI which has been
supplied in solid form? And the mixing proportion.All recommendation
welcome.

thank you
Foo Chin Peng
Nanyang Technological University
email -  [email protected]