A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: List of attacked/etched materials
List of attacked/etched materials
2009-11-06
[email protected]
2009-11-06
Loren St. Clair
2009-11-06
antwi nimo
2009-11-07
Edward Sebesta
List of attacked/etched materials
antwi nimo
2009-11-06
http://en.wikibooks.org/wiki/Microtechnology/Etching_Processes

I hope this links helps,
regards.


--- On Fri, 11/6/09, [email protected]  wrote:

From: [email protected] 
Subject: [mems-talk] List of attacked/etched materials
To: [email protected]
Date: Friday, November 6, 2009, 6:41 AM

Hi,

I am looking for papers/books/publications stating which metal is
etched/attacked/not attacked by the most common etchants (mainly HF, HCl,
H2O2, citric acid, phosphoric acid). Furthermore I'd like to find also
information about attack of some common semiconductors and oxides (like
GaAs, Si, Al2O3, SiO2, HfO2).

I could only find books showing which etchant etches BEST which metal - like
the book 'Advanced Inorganic Chemistry' of F. Cotton. But I need to know if
there is non/some/a lot of attack of a material. E.g. is Nickel totally
stable in HCl, Cr in HF etc., or is there a considerable attack?

Thanks in advance
Daniel
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group