Hello all,

I need to etch Silicon isotropically to create a hemisphere shape.
Thus, I need to know how smooth DRIE can etch the surface of Silicon about
100 microns.
Is anyone know the surface roughness that DRIE etches the silicon down to
100 microns?
Plus, Do you know that DRIE isotropic etching will form a negative
hemispherical shape?


Thank you


Jiho Song
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group
MEMStaff Inc.