MEMSnet Home: MEMS-Talk: Moisture in PDMS
Moisture in PDMS
2009-11-25
A. AhmadShukri
2009-11-26
Gareth Jenkins
2009-11-27
Bill Moffat
Moisture in PDMS
Gareth Jenkins
2009-11-26
Modest heating and/or vacuum shouldn't significantly alter it's properties.

On Wed, Nov 25, 2009 at 16:54, A. AhmadShukri wrote:

> Dear all,
>
> I am using water droplets on PDMS surface and am wondering water could be
> trapped between my features on the PDMS. If so, is there a way to
> dehumidify
> PDMS without altering its properties?
>
> Thanks,
> Aimi
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Harrick Plasma, Inc.
MEMS Technology Review