MEMSnet Home: MEMS-Talk: RE: Electrodeposited photoresists
RE: Electrodeposited photoresists
1998-10-27
Roberto Igal Chertkow
1998-10-27
Matthias Heschel
RE: Electrodeposited photoresists
Roberto Igal Chertkow
1998-10-27
Dear sir,
I a time ago needed a electrodeposited PHR.
I found that Shipley has such material named EAGLE.

you may contact

Kevin Smith
Shipley House, Herald Way, Coventry CV3 2RQ, UK
Tel. 01203 457203
Fax 01203 440331
Telex 311316


All the best,

Igal Chertkow


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
The Branford Group
Mentor Graphics Corporation