MEMSnet Home: MEMS-Talk: thick structurable films
thick structurable films
2009-12-04
Mikael Evander
2009-12-05
Bob Henderson
2009-12-05
Mikael Evander
2009-12-05
Brian Stahl
thick structurable films
Mikael Evander
2009-12-05
Hi Bob.

Doesn't SU-8 require an additional spun-on layer of SU-8 in order to bond
after developing? I was looking at SU-8 from the beginning but couldn't
find a decent way of bonding the structured/developed SU-8 to the second
glass wafer? I'm looking at a glass - SU-8 - glass structure.

Thanks!

/Mikael

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Bob Henderson
Sent: Friday, December 04, 2009 3:20 PM
To: 'General MEMS discussion'
Subject: Re: [mems-talk] thick structurable films

Try SU-8
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Mentor Graphics Corporation
Harrick Plasma, Inc.