Hi,
    I am trying to deposit metal on SiN membrane windows after lithography and
want to perform liftoff. But seems it is very hard to remove resist enen
overnight soaking in PG remover. Since membrane is only around 50 nm thick, and
I can't not use ultrasonic bath because it will break membrane.  I even have
trouble in using N2 blow to dry membrane wafers. Does anyone have any experience
how to do it on membrane?

Thanks

Xiaoyong

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Mentor Graphics Corporation
Nano-Master, Inc.