A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: silicon membranes
silicon membranes
2009-12-20
Andrea Mazzolari
2009-12-21
Kuijpers, Peter
2009-12-21
Nathan McCorkle
2009-12-21
Morten Aaroe
2009-12-21
Brian Stahl
2009-12-22
Albert Henning
2009-12-23
Chilcott, Dan - NV
2009-12-24
Andrea Mazzolari
2009-12-25
Andrea Mazzolari
2009-12-28
Albert Henning
2009-12-28
Albert Henning
silicon membranes
Albert Henning
2009-12-28
The fracture strength of a 30 um membrane which is 5x5 mm^2 should be
high enough that you don't have to be ultra-careful (but, still, be
careful!); it should be over 100 psid.  I don't have the equations right
at my desk, but feel free to email me if you'd like to know more exact
estimates of fracture strength from my experience with similar
membranes.

Kirt is right about depletion, but there could also be a stress effect
during the initial etching; although I did not experience this effect.
Did you measure the stress in your nitride film?

Al

---
Albert K. Henning, PhD
Director of MEMS Technology
NanoInk, Inc.
215 E. Hacienda Avenue
Campbell, CA  95008
408-379-9069  ext 101
[email protected]

-----Original Message-----
From: Andrea Mazzolari [mailto:[email protected]]
Sent: Friday, December 25, 2009 1:58 AM
To: [email protected]
Cc: 'General MEMS discussion'
Subject: Re: [mems-talk] silicon membranes

Hi Kirt,

i already tried adding Sb2O3 as surfactant, surfaces were mirror like,
so surfactant was working well.

Agitation was realized with a magnetic stirrer, but was not so strong.
I'm afraid that strong agitation may destroy membranes.
Ok, if etching at room temperature will not work i will try with
ultrasound.

In any case i need to realize just 4-5 membranes, and i have a lot of
time to realize them, so i can accept to realize etching at room temperature.

Best regards,
Andrea
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
MEMStaff Inc.
Harrick Plasma, Inc.