Hello,

Petrol deformed microfluidic PDMS structure, it also depends on the UV cured
PDMS substrate condition.


Mamun Rashid
Research Assistant
Centre for Nano & Microsystems
University of Teesside
TS1 3BA. U.K
+44(0)164 234 2428


________________________________________
From: [email protected] [[email protected]] On Behalf Of
闫许 [[email protected]]
Sent: 04 January 2010 01:47
To: [email protected]
Subject: [mems-talk] Does petrol swell or etch PDMS?

Dear all,

       I would like to protect my chip immerged in petrol using PDMS film.
Does petrol swell or etch PDMS?

       Thanks a lot!

X. Yan
Shanghai Institute of Microsystem And Information Technology
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation