Dear Everyone,

Need help:

1\ after soft bake, i will see some bubbles inside of SU8 film, does it have
some bad effect?

2\ Could you give me some suggestion about developing SU8?
I use BTS-220 now, after developing, my figure are not swelling, but will
adhere with each other when the distance is so small(~2um). I think maybe I
do something wrong in develop step.

Peng Xu
University of Louisville
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Process Variations in Microsystems Manufacturing
The Branford Group