A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Transparent conductive coating
Transparent conductive coating
2010-01-06
Brad Cantos
2010-01-06
DongJuan Xi
2010-01-07
Gareth Jenkins
2010-01-07
Kevin Paul Nichols
2010-01-07
Brad Cantos
2010-01-07
DongJuan Xi
2010-01-07
David Casale
Transparent conductive coating
David Casale
2010-01-07
Hi Brad,

ITO would be the way to go. You can go more conductive than that with
ITO without too many problems, on glass at least. The adhesion to
something like PI is probably good, but it depends on your plastic and
how adherent coatings are to it in general, as well as the roughness,
etc, as that can have an effect on adhesion and sheet resistance.

Sincerely,
David Casale
www.maxlevy.com




-----Original Message-----
From: Brad Cantos [mailto:[email protected]]
Sent: Wednesday, January 06, 2010 11:42 AM
To: General MEMS discussion
Subject: [mems-talk] Transparent conductive coating

Hi Everyone, and Happy New Year.

Is anyone aware of a service that can apply a transparent conductive
coating to a plastic sheet?  This would have to be fairly low
temperature process due to the low melting point of the plastic.  The
sheet resistance requirements are not too rigorous, anything under 400
ohms/square should be fine.  Optimally, it would need to be >99%
transmissive over 400-1100nm wavelength range, but at this point >80% is
acceptable.

Thanks for your help.

Brad Cantos
[email protected]
http://holage.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
University Wafer
Harrick Plasma, Inc.