A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: protecting layer/material during KOH Si etching forSiN membrane formation
protecting layer/material during KOH SiN membrane formation
2010-01-07
Xiaoyong Liu
protecting layer/material during KOH Si etching forSiN membrane formation
2010-01-12
Morrison, Richard H., Jr.
2010-01-08
Karolina psychowlosy
protecting layer/material during KOH Si etching forSiN membrane formation
Morrison, Richard H., Jr.
2010-01-12
You can use black wax Apiezon.

Rick


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Xiaoyong Liu
Sent: Thursday, January 07, 2010 3:08 PM
To: [email protected]
Subject: [mems-talk] protecting layer/material during KOH Si etching
forSiN membrane formation

Hi All,

      I am in a processing of making SiN membrane by using KOH chemical
etching on SiN(~50nm) coated Si wafers. There are some patterns on one
side of wafer, and I want them intact during KOH etching. The total
etching time will be about 5-6 hours.  I am wondering if there is any
material/film I can put on to protect that side of wafer, and can be
readily removed afterwards.

Thanks a lot

Xiaoyong
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMStaff Inc.