Wet etching gold
2010-01-12
delas lee
2010-01-12
Bill Moffat
2010-01-12
mikas remeika
Wet etching gold
Bill Moffat
2010-01-12
Metal lift off leaves metal where you want and none where you want none.
Contact me for a number of technical papers at
[email protected].  Bill Moffat.

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of delas lee
Sent: Tuesday, January 12, 2010 6:34 AM
To: [email protected]
Subject: [mems-talk] Wet etching gold

Hello;

I tried to make wet etching of gold evaporated on thin layer of Titanium
on Polymer substrate.

But the gold layer don't stick very well on substrate, because after
etching with cyanides, it remove all the gold on surface substrat even
that covered by sacrifice layer.

I am looking for a process that leaving gold sticks very well on polymer
substrate.

Thank you for your time.

DELAS Lee
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
MEMS Technology Review
Mentor Graphics Corporation