MEMSnet Home: MEMS-Talk: roughening boro glass surface
roughening boro glass surface
2010-01-13
RS Forman
2010-01-13
Mikael Evander
roughening boro glass surface
Mikael Evander
2010-01-13
I think I've read about the use of phosphoric acid but I'm not sure if
that also only applies to soda lime glass. Might be worth looking into?

/mikael

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of RS Forman
Sent: Wednesday, January 13, 2010 12:19 PM
To: [email protected]
Subject: [mems-talk] roughening boro glass surface

I am looking for a wet chemical formula that will roughen borosilicate
glass.  I have used HF + biflorides to get a very frosty surface on soda
lime glass, but cannot get the same effect on borosilicate glass.. any
ideas?

Thanks,  Robert
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
University Wafer
MEMS Technology Review