A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Lift-off pattern of Cu or Ni film
Lift-off pattern of Cu or Ni film
2010-01-13
leiwangsdu
2010-01-14
Bill Moffat
Lift-off pattern of Cu or Ni film
leiwangsdu
2010-01-13
I'm a research fellow. I have a question about lift-off process of Cu or Ni.
Is it possible to fabricate a pattern of Cu or Ni film with nearly steep
sidewall.
The thickness of Cu or Ni is 3-4 microns. If anyone knows, please tell me
the method and the necessary process.