Hi All,

i need to realize (110) oriented vertical sidewalls in (110) silicon wafers.
I've found that addition of IPA to KOH changes the etch rates and should
provide this result. I do not have any information on the needed IPA
quantity to be addeded to the solution.

Any suggestion, please ?

Thanks,
Andrea