MEMSnet Home: MEMS-Talk: Piranha Reaction
Piranha Reaction
2010-01-26
DEBASHIS MAJI
2010-01-27
Roger Brennan
2010-01-27
Edmondo Battista
Piranha Reaction
DEBASHIS MAJI
2010-01-26
Dear all,

I shall be highly thankful if anyone can kindly tell the effect of change in
the ratio of H2O2 and H2SO4 (normally 1:1) in Piranha solution. I know that
this reaction takes place in the following order : H2O2 + H2SO4 = HSO4(-) +
H3O(+) + O. It is this nascent oxygen that is used in cleaning or surface
treatment, etc. I would like to know the effect of increase in sulphuric
acid conc. say from 1:1 to 3:1 in the piranha solution. Would it result in
more vigorous reaction with more nascent O? if so how do the equations
go...?

Kindly help me out regarding this. Thanks in advance.

Debashis Maji,
JRF - Texas Instruments & IIT Kharagpur collaborative Project,
PhD Scholar - School of Medical Science & Technology,
IIT Kharagpur, India - 721302
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Nano-Master, Inc.