MEMSnet Home: MEMS-Talk: 1165 and GaAs compatibility?
1165 and GaAs compatibility?
2010-01-27
mikas remeika
2010-01-27
Andy Irvine
2010-01-28
Morrison, Richard H., Jr.
1165 and GaAs compatibility?
Morrison, Richard H., Jr.
2010-01-28
I used 1165 with GaAs wafers and I never had an issue, 1165 is mostly
NMP (solvent) I do not think it attackts 1165.

Rick


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of mikas remeika
Sent: Wednesday, January 27, 2010 2:36 PM
To: General MEMS discussion
Subject: [mems-talk] 1165 and GaAs compatibility?

In a recent post it was mentioned the Microposit 1165 attacks GaAs at
some slow rate. Could anyone share their specific experiences
regarding this? I.e. under what conditions the etch might occur and
approximately what etch rate is expected? This is very worrying to me
since the spec sheet seems to imply that 1165 is GaAs compatible.

Also, what about Remover PG ? Are there any known semiconductors that
it attacks?

thank you,
-mikas
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMStaff Inc.
Nano-Master, Inc.