Hi all,

I would like to know whether anybody has any information regarding surface
treatment of PDMS with piranha solution. Also is it as effective as plasma
treatment? I shall be highly obliged if anyone can help me out in this and
provide some material.

Thanks in advance.

Debashis Maji,
JRF - Texas Instruments & IIT Kharagpur collaborative Project,
PhD Scholar - School of Medical Science & Technology,
IIT Kharagpur, India - 721302
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Addison Engineering
Mentor Graphics Corporation