 Hi All,

I would like to use a micro moulding technique to cast a pattern into spun on
polyurethane.  I wanted to used a rigid material to pattern the negative easier
to align. I was thinking of SU-8 using photolithography but I am not sure if the
polyurethane would just simply peel of this.  Another other suggestions of
photoresists that would not adhere to polyurethane (PMC-790 by Smooth on)

Darren Alvares
Post-Graduate Student
Graduate School of Biomedical Engineering
 University of New South Wales
UNSW Sydney NSW 2052 Australia
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
MEMStaff Inc.
Harrick Plasma, Inc.