MEMSnet Home: MEMS-Talk: Help for photoresist coating
Help for photoresist coating
2010-02-11
leiwangsdu
2010-02-11
Felix Lu
2010-02-11
Javier Sesé
2010-02-11
mikas remeika
2010-02-11
Y.Tian
2010-02-11
Robert Black
2010-02-11
Mathai, Sagi
2010-02-11
Robert MacDonald
2010-02-12
Bill Moffat
Help for photoresist coating
Robert Black
2010-02-11
Increasing the temp of the resist will increase the thickness at the center.
Lowering the exhaust( if you have exhaust) will lower the thickness at the
edge. Are you doing an EBR (edge bead removal)? May be hard to do on a
rectangle though.


Robert

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Y.Tian
Sent: Thursday, February 11, 2010 9:07 AM
To: General MEMS discussion
Subject: Re: [mems-talk] Help for photoresist coating

It is normal to have resist thicker near the edge than the centre, that's
the physics of the spin coating. You can not completely avoid it. What I can
suggest, you can try to leave the sample on a nice flat surface for few
minutes once you done the spin coating. Bear in mind the photoresist is a
kind of liquid anyway, this will allow part of the liquid flow back from the
edge to the central part. Then you can do the baking afterwards. The other
thing is your sample is so small, why don't you try to spinning coating a
larger area then dice into smaller pieces?

Yingtao
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.