Wet-chemical etching of Au without etching Al
2010-02-15
Lisa Gades
2010-02-16
Dave Lewis
2010-02-16
Andy Irvine
2010-02-16
Dave Lewis
2010-02-16
Kevin Paul Nichols
2010-02-16
David Roberts
2010-02-17
Lisa Gades
2010-02-17
David Springer
2010-02-19
Lisa Gades
Wet-chemical etching of Au without etching Al
Lisa Gades
2010-02-19
Hi David,

We are not at all committed to using Au; in fact, we had tried Cr
first.  Thank you for your suggestions of other metals to try with a dry
etch process.

Thanks again to everyone for your helpful suggestions!  We have several
avenues to try.

Lisa
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
The Branford Group
MEMS Technology Review