MEMSnet Home: MEMS-Talk: Al thin film dissolved inside hot water
Al thin film dissolved inside hot water
2010-02-18
li shifeng
2010-02-19
David Casale
2010-02-22
Morrison, Richard H., Jr.
Al thin film dissolved inside hot water
David Casale
2010-02-19
Hi Shifeng,

This is something easy to forget, but diffusion is length^2/time, and at
really short length scales and moderate temperatures, diffusion can be
pretty "big". I'd guess that it is diffusing off of the surface and into
solution, but I haven't tried to look at any data to verify that. Try
lower temperature water, and see if it takes longer to dissolve, and you
problem will be pretty obvious.

As an example, mild temperatures can fully diffuse adhesion layers into
top layers with thin films (say 150 angstroms of Cr under 2000 angstroms
of Au), and it is a very complicated process to prevent this diffusion.
At say 300C and a few hours of soak time, on glass, Cr will diffuse
completely into Au if the length scales are small enough and grain
structure right. Easy experiment to perform if you do it on glass too,
just look through the back side at the adhesion layer of different
color, no fancy equipment.

I have some sources for this as well if you decide this is your problem,
or want to look more into it.

Sincerely,
David Casale

-----Original Message-----
From: li shifeng [mailto:[email protected]]
Sent: Thursday, February 18, 2010 12:53 PM
To: [email protected]
Subject: [mems-talk] Al thin film dissolved inside hot water

Hi All,

I deposited 70nm - 80nm Al thin film on the glass coverslips with and
without any adesion layer. I found Al thin film was dissolved inside hot
water Note: 90C) after 30 mins to 45mins. This really bothered me quite
a bit. What are the possible reasons for this and how to solve this
problem?

Thanks!

Shifeng
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Nano-Master, Inc.
MEMS Technology Review