SiGe deposition
Ned Flanders
2010-02-20
Hi Andrea,

Would you be so kind and get back to us when you find some useful
references? That is, could you please post here the articles you found
most helpful to you?

Thanks in advance

m

On 2/19/10, Andrea Mazzolari  wrote:
> Hi Wendell,
>
> here we have our own LEPECVD system. I'm just new to this machine,
> I simply want to learn to use it.
>
> My understanding is this mailing list is a good opportunity to share our
> experiences, not to find someone who will realize the work for me.
>
> Best regards,
> Andrea
>
>
> > Andrea,
> >
> >       As others here have indicated this is not like falling off a log.
> > Those who are doing it successfully have put a LOT of engineering into it.
> > Send me an E-mail directly and I can connect you with a vendor that can do
> > the job for you.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Mentor Graphics Corporation