Hello all,

I was wondering if any of you have worked on etching Ni-Fe. I am currently
using Ni Etchant type 1 from Transene and it gives huge undercut during
etching. Undercut is close to 10 times the actual thickness to be etched.
Does anyone have experience etching Ni-Fe with any other etchant with
minimal undercut?

Thanks,

Pavan Samudrala
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.