In my experience etching copper, which can also suffer from severe undercut,
diluting the etchant significantly along with mild agitation reduced
undercuts from ~10x to ~3x.

Regards,
Greg Ostrowicki


On Wed, Mar 17, 2010 at 3:46 PM, Pavan Samudrala
wrote:

> Hello all,
>
> I was wondering if any of you have worked on etching Ni-Fe. I am currently
> using Ni Etchant type 1 from Transene and it gives huge undercut during
> etching. Undercut is close to 10 times the actual thickness to be etched.
> Does anyone have experience etching Ni-Fe with any other etchant with
> minimal undercut?
>
> Thanks,
>
> Pavan Samudrala
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.