A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Cleaning optical masks
Cleaning optical masks
2010-03-26
mikas remeika
2010-03-26
Le Cao Hoai Nam
2010-03-26
Andrew Irvine
2010-03-26
Le Cao Hoai Nam
2010-03-26
郑瑞麟(Ruilin Zheng)
2010-03-26
Ruiz, Marcos Daniel (SENCOE)
2010-03-26
Joseph Grogan
2010-03-26
shay kaplan
2010-03-26
Mike Whitson
2010-03-26
Miyakawa, Natsuki
2010-03-26
Elina Kasman
Cleaning optical masks
Le Cao Hoai Nam
2010-03-26
Hi Mikas,

You can easily clean the mask with hot Piranha bath (110C) for 15 min.
You should use a big quartz beaker and put the soda-lime glass side of
the mask downward to the quartz beaker and the Cr side of the mask
upward. I don't know how robust is your mask so you should test first
by dipping a small corner of the mask to the Piranha bath. I cleaned
our masks (Cr in soda-lime glass) several times with Piranha bath and
there was no problem.

Greetings,

Nam
Dublin City University

On Fri, Mar 26, 2010 at 12:50 AM, mikas remeika
 wrote:
> Dear, Everyone,
>
> I have a photolitography mask, that is starting to accumulate stains
> of SU-8, from the many times it was in contact with samples.  For
> other resists its usually sufficient to rinse the mask in acetone, but
> SU-8 is resistant to most solvents after numerous exposures to UV
> light. I was thinking of trying an oxygen asher. It seems like that
> should be ok, but, just in case, are there are reasons to avoid
> exposing such masks to oxygen plasma? The mask is Soda-Lime coated
> with Cr.
>
> thank you,
> -Mikas
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
University Wafer
Tanner EDA by Mentor Graphics