A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Cleaning optical masks
Cleaning optical masks
2010-03-26
mikas remeika
2010-03-26
Le Cao Hoai Nam
2010-03-26
Andrew Irvine
2010-03-26
Le Cao Hoai Nam
2010-03-26
郑瑞麟(Ruilin Zheng)
2010-03-26
Ruiz, Marcos Daniel (SENCOE)
2010-03-26
Joseph Grogan
2010-03-26
shay kaplan
2010-03-26
Mike Whitson
2010-03-26
Miyakawa, Natsuki
2010-03-26
Elina Kasman
Cleaning optical masks
Ruiz, Marcos Daniel (SENCOE)
2010-03-26
We have experience problems using O2 ashers on chrome.  Be careful.

Dan

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf
Of Andrew Irvine
Sent: Friday, March 26, 2010 7:04 AM
To: General MEMS discussion
Subject: Re: [mems-talk] Cleaning optical masks

Just to re-visit a wise warning from a recent poster, Piranha etch (at
110C or not) is seriously hazardous, and we need to be flagging up
safety advice when suggesting stuff.

I don't see a problem with using an oxygen asher, and if there is no
problem (anyone?), do that instead, Mikas!

Andy
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange