Best way to spin PDMS for making sheets?
2010-03-27
Nathan McCorkle
2010-03-27
Kevin Paul Nichols
2010-03-28
Nathan McCorkle
2010-03-28
Bill Moffat
2010-03-28
Harsh Sundani
2010-03-29
Nathan McCorkle
2010-03-29
Kevin Paul Nichols
2010-03-29
Nathan McCorkle
Best way to spin PDMS for making sheets?
Nathan McCorkle
2010-03-27
I am using a laser to ablate PDMS to make channels. I tried peeling
off the PDMS layer, but it was attached quite well to both polished
aluminum wafers as well as silicon wafers. I am not sure what the best
method of getting the PDMS to release will be, please help!

-Nathan McCorkle
---
Rochester Institute of Technology
College of Science, Biotechnology/Bioinformatics
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Harrick Plasma, Inc.
Addison Engineering