A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Etching SOI wafer from back side
Etching SOI wafer from back side
2010-05-05
weiquan yang
2010-05-05
QAZI, MUHAMMAD
2010-05-05
Kagan Topalli
2010-05-06
Om Suwal
2010-05-06
weiquan yang
2010-05-07
Massimiliano Decarli
2010-05-06
M. Emre Karagozler
2010-05-07
Brian Stahl
2010-05-07
Jie Zou
Etching SOI wafer from back side
weiquan yang
2010-05-05
I want to etch away the Si base substrate of SOI wafer from back side and
remain the top thin Si layer and buried oxide layer.  I try the wet etching
in both ways (using TMAH or KOH solution). The SiO2 or Si3N4 deposited by
PECVD were used as protection mask layers (both side: top and back). However
SiO2 or Si3N4 can not survive very well in the hot sulution for long term
(several hours). Some local areas of top Si layer of SOI was etched
away. Could you guys kindly give me some suggestions? Is this due to the
quality of SiO2 or Si3N4 layer? The quality of SiO2 or Si3N4 by PECVD may be
not very good , so the SiO2 or Si3N4 can not survive.
Some dry etching suggestion is aslo welcome.

Thank you!

Weiquan Yang
EE department
University of Texas at Arlington
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group